Compressive Yield Strength 390 MPa

@Temperature 130 °C
56600 psi

@Temperature 266 °F
90º, Wet; EN2850 Type B
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber
Information provided by HexCel
Compressive Yield Strength 390 MPa
56600 psi
ASTM D695
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin