Polymer Property : Compressive Yield Strength = 53100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 366 MPa

@Temperature 23.0 °C
53100 psi

@Temperature 73.4 °F
Hexcel® HexPly® 954-3 Curing Cyanate Resin, K13C-2U Fiber
Information provided by HexCel