Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 366 MPa @Temperature 23.0 °C |
53100 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-3 Curing Cyanate Resin, K13C-2U Fiber Information provided by HexCel |