Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 47.6 - 52.4 MPa | 6900 - 7600 psi | Average value: 49.1 MPa Grade Count:4 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |