Mechanical Properties Metric English Comments
Compressive Yield Strength 0.340 MPa
49.3 psi
at 10% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ F DF-630A Closed Cell Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 75Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Compressive Yield Strength 0.340 MPa
49.3 psi
at 10% Compression, Parallel to thickness
Zircar Ceramics ECO-27A Alumina-Silica Insulation
This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer..
Compressive Yield Strength 0.340 MPa
49.3 psi
Compressive Load Deflection at 5%; ASTM D575
Aearo E-A-R Specialty Composites VersaDamp™ V-2750 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..