Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.340 MPa | 49.3 psi | at 10% deflection; ASTM D3574C |
Mearthane Durethaneâ„¢ F DF-630A Closed Cell Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 75Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
Compressive Yield Strength | 0.340 MPa | 49.3 psi | at 10% Compression, Parallel to thickness |
Zircar Ceramics ECO-27A Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer.. |
|||
Compressive Yield Strength | 0.340 MPa | 49.3 psi | Compressive Load Deflection at 5%; ASTM D575 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2750 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |