Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 33.0 - 145 MPa | 4790 - 21000 psi | Average value: 73.9 MPa Grade Count:12 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Compressive Yield Strength | 33.0 - 148 MPa | 4790 - 21500 psi | Average value: 87.0 MPa Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |