Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 474 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 474 MPa

@Temperature 23.0 °C
68700 psi

@Temperature 73.4 °F
Open Hole
Hexcel® HexPly® M36/NC2 180°C (350°F) Curing Epoxy Matrix, Multiaxial Fabric Laminate (NC2)
Uses Hexcel NC2 non-crimp fabric based on Tenax HTS fiber; Quasi-isotropic lay-up based on 1072 gsm quadaxial NC2 fabric (267 gsm/ply); Laminates manufactured via resin film infusionInformation prov..