Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 47.0 MPa @Strain 25.0 % |
6820 psi @Strain 25.0 % |
Z direction; 0.05/min strain rate; ASTM D695 |
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight .. |