Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 32.30 MPa | 4685 psi | ASTM D695 |
Protective Coating PC-Clear™ Clear Liquid Epoxy PC-Clear™ is a completely clear liquid epoxy formulated to remain clear during and after its curing time. PC-Clear™ is very durable and flexible making it unlike many liquid epoxies. Uses include.. |