Protective Coating PC-Clear™ Clear Liquid Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Protective Coating Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Protective Coating PC-Clear™ Clear Liquid Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC-Clear™ is a completely clear liquid epoxy formulated to remain clear during and after its curing time. PC-Clear™ is very durable and flexible making it unlike many liquid epoxies. Uses include repairs needing to be disguised or repairs requiring the absence of color. PC-Clear™ demonstrates excellent chemical resistance to mild acids, caustics, detergents, gasoline, fuel oil, salt, and fresh water.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
1 Week Cure; ASTM D2240
Elongation at Break 2.0 %
2.0 %
Flexural Strength 20.1 MPa
2920 psi
ASTM D580
Compressive Yield Strength 32.30 MPa
4685 psi
ASTM D695
Shear Strength 15.9 MPa
2300 psi
Tensile Shear Strength; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Thickness Not Known
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
Tack Free
60.0 min
1.00 hour
For Service
1440 min
24.0 hour
Max Cure
Pot Life 4.0 min

@Temperature 21.1 °C
4.0 min

@Temperature 70.0 °F
Working Time
Descriptive Properties Value Comments
Color Clear
Component A
Clear
Component B
Clear
Mixed
Thermal Shock Resistance Excellent
Toxicity Nontoxic after cure