Polymer Property : Compressive Yield Strength = 45500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 100 - 314 MPa
14500 - 45500 psi
Average value: 186 MPa Grade Count:33
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Compressive Yield Strength 159 - 314 MPa
23100 - 45500 psi
Average value: 213 MPa Grade Count:7
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..