Mechanical Properties Metric English Comments
Compressive Yield Strength 100 - 314 MPa
14500 - 45500 psi
Average value: 186 MPa Grade Count:33
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Compressive Yield Strength 100 - 207 MPa
14500 - 30000 psi
Average value: 155 MPa Grade Count:4
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Compressive Yield Strength 100 - 234 MPa
14500 - 33900 psi
Average value: 200 MPa Grade Count:21
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum ..
Compressive Yield Strength 100 - 179 MPa
14500 - 26000 psi
Average value: 150 MPa Grade Count:10
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Compressive Yield Strength 100 MPa
14500 psi
ISO 14126
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP
SMC 0400 is a Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to parts with good up to excellent surface quality for medium bake in-line and off-line p..
Compressive Yield Strength 100 MPa
14500 psi
ISO 14126
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP
SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain..
Compressive Yield Strength 100 MPa
14500 psi
"ab" direction
Momentive Performance Materials "PG" Pyrolytic Graphite
Pyrolytic Graphite (PG) is a unique form of graphite manufactured by decomposition of a hydrocarbon gas at very high temperature in a vacuum furnace. The result is an ultra-pure product which is ne..
Compressive Yield Strength 100 MPa
14500 psi
ISO 14126
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP
SMC 0412 is a premium Class-A SMC for on-line painted conductive exterior body applications on cars. These compounds mould to parts with excellent surface quality and low surface conductivity for e..
Compressive Yield Strength 100 MPa
14500 psi
ASTM D695
Westlake Plastics Polyethersulfone
High resistance to heat and combustibility, low smoke emission, and transparency are the combination of properties possessed by stock shapes extruded from PES. These, coupled with light weight, good..
Compressive Yield Strength 100 - 241 MPa
14500 - 35000 psi
Average value: 133 MPa Grade Count:25
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Compressive Yield Strength 100 - 117 MPa
14500 - 17000 psi
Average value: 111 MPa Grade Count:3
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..