Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 30.1 MPa | 4370 psi | at 10% deflection, parallel to thickness |
Zircar Refractory Composites RS-99R Refractory Sheet Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI) |