Polymer Property : Compressive Yield Strength = 30.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 30.1 MPa
4370 psi
at 10% deflection, parallel to thickness
Zircar Refractory Composites RS-99R Refractory Sheet
Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)