Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 291 MPa | 42200 psi | Compression strength after impact, 6J |
Hexcel® HexPly® M36/NC2 180°C (350°F) Curing Epoxy Matrix, Multiaxial Fabric Laminate (NC2) Uses Hexcel NC2 non-crimp fabric based on Tenax HTS fiber; Quasi-isotropic lay-up based on 1072 gsm quadaxial NC2 fabric (267 gsm/ply); Laminates manufactured via resin film infusionInformation prov.. |