Mechanical Properties Metric English Comments
Compressive Yield Strength 172 - 379 MPa
25000 - 55000 psi
Average value: 234 MPa Grade Count:13
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma..