Polymer Property : Compressive Yield Strength = 3480 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 24.0 MPa

@Strain 1.00 %
3480 psi

@Strain 1.00 %
ISO 604
Manifattura Cattaneo PA 6 Nylon
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Compressive Yield Strength 24.0 MPa

@Strain 1.00 %
3480 psi

@Strain 1.00 %
ISO 604
Manifattura Cattaneo PET+PTFE Polyethylene Terephthalate
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Compressive Yield Strength 24.0 - 120 MPa
3480 - 17400 psi
Average value: 61.6 MPa Grade Count:7
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..