Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 22.8 MPa | 3300 psi | Stabilized |
Hexcel® HexWeb® HDC - 3/16 - 16.0 (R2) Heavy Density Core Designation: Material-Cell Size (inches)-DensityHexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with eit.. |