Mechanical Properties Metric English Comments
Compressive Yield Strength 22.8 MPa
3300 psi
Stabilized
Hexcel® HexWeb® HDC - 3/16 - 16.0 (R2) Heavy Density Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with eit..