Polymer Property : Compressive Yield Strength = 29600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 204 MPa
29600 psi
Compression After Impact, 30J
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix, Unidirectional Prepreg Laminate (M36/32%/135/HTA)
Tenax HTA fiberInformation provided by HexCel
Compressive Yield Strength 204 MPa

@Strain 10.0 %,
Temperature 23.0 °C
29600 psi

@Strain 10.0 %,
Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 4211 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..