Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 204 MPa | 29600 psi | Compression After Impact, 30J |
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix, Unidirectional Prepreg Laminate (M36/32%/135/HTA) Tenax HTA fiberInformation provided by HexCel |
|||
Compressive Yield Strength | 204 MPa @Strain 10.0 %, Temperature 23.0 °C |
29600 psi @Strain 10.0 %, Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 4211 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |