Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 180 MPa | 26100 psi | ISO 14126 |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Compressive Yield Strength | 180 MPa | 26100 psi | ASTM D695 |
Sumitomo Bakelite North America FS-10-VO-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Compressive Yield Strength | 180 MPa | 26100 psi | ISO 604 |
Hexcel® HexPly® 914 175°C Curing Epoxy Matrix HexPly® 914 is a highly successful modified epoxy matrix which is used extensively in high temperature resistant primary aircraft structures. The controlled melt viscosity and excellent matrix rheo.. |
|||
Compressive Yield Strength | 180 MPa @Temperature 23.0 °C |
26100 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-6 Curing Cyanate Resin HexPly® 954-6 is a 250°F (121°C) curing toughened cyanate resin with 300°F (149°C) Tg. HexPly® 954-6 is formulated for autoclave curing. Recommended cure is three hours at 250°F (121°C). Ser.. |