Mechanical Properties Metric English Comments
Compressive Yield Strength 180 MPa
26100 psi
ISO 14126
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP
SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel..
Compressive Yield Strength 180 MPa
26100 psi
ASTM D695
Sumitomo Bakelite North America FS-10-VO-P Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI..
Compressive Yield Strength 180 MPa
26100 psi
ISO 604
Hexcel® HexPly® 914 175°C Curing Epoxy Matrix
HexPly® 914 is a highly successful modified epoxy matrix which is used extensively in high temperature resistant primary aircraft structures. The controlled melt viscosity and excellent matrix rheo..
Compressive Yield Strength 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
Hexcel® HexPly® 954-6 Curing Cyanate Resin
HexPly® 954-6 is a 250°F (121°C) curing toughened cyanate resin with 300°F (149°C) Tg. HexPly® 954-6 is formulated for autoclave curing. Recommended cure is three hours at 250°F (121°C). Ser..