Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 100 - 234 MPa | 14500 - 33900 psi | Average value: 200 MPa Grade Count:21 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Compressive Yield Strength | 155 - 234 MPa | 22500 - 33900 psi | Average value: 208 MPa Grade Count:31 |
Overview of materials for Phenolic, Novolac, Woodflour Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu.. |