Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 156 - 410 MPa | 22600 - 59500 psi | Average value: 250 MPa Grade Count:23 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Compressive Yield Strength | 155.8 MPa | 22600 psi | ASTM D695 |
Plenco 51015 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by.. |