Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 5.00 - 15.2 MPa | 725 - 2200 psi | Average value: 7.11 MPa Grade Count:6 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Compressive Yield Strength | 5.00 - 15.2 MPa | 725 - 2200 psi | Average value: 6.57 MPa Grade Count:9 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |