Compressive Yield Strength 0.152 MPa
22.0 psi
at 25% deflection; ASTM D1056
Rogers Corporation Bisco™ HT-840 Cellular Silicone Foam
Extra firm grade silicone sponge. UL recognized of flame retardance.Applications: High closure-force gaskets, Press-pads where conformable imprinting support is required, such as decal lamination o..