Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.152 MPa | 22.0 psi | at 25% deflection; ASTM D1056 |
Rogers Corporation Bisco™ HT-840 Cellular Silicone Foam Extra firm grade silicone sponge. UL recognized of flame retardance.Applications: High closure-force gaskets, Press-pads where conformable imprinting support is required, such as decal lamination o.. |