Polymer Property : Compressive Yield Strength = 21200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 146 MPa
21200 psi
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex
Compressive Yield Strength 146 MPa
21200 psi
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix
HexPly® M36 is a high performance 180ºC cure matrix developed for aerospace and industrial markets. It can be used in a variety of production techniques (Resin Film Infusion (RFI), prepreg and sem..