Compressive Yield Strength 20.0 MPa
2900 psi
Stabilized, typ
Hexcel® HexWeb® CR III 1/8-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Yield Strength 20.0 MPa
2900 psi
Stabilized, typ
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.0037 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Compressive Yield Strength 20.0 - 103 MPa
2900 - 14900 psi
Average value: 59.2 MPa Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Compressive Yield Strength 20.0 MPa

@Strain 1.00 %
2900 psi

@Strain 1.00 %
ISO 604
Manifattura Cattaneo POM c+PTFE Acetal, PTFE Filled