Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 17.4 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.120 MPa
17.4 psi
at 30% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ M DM-715A Foam Polyurethane
MDI backbone: ether.Shore 00 Hardness: 60Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
Compressive Yield Strength 0.120 MPa
17.4 psi
at 10% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ F DF-235A Closed Cell Foam Polyurethane
TDI backbone: ester.Shore 00 Hardness: 80Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Compressive Yield Strength 0.120 - 0.170 MPa
17.4 - 24.7 psi
25% Compression
BIW ASTM Class 2D5 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...
Copyright © lookpolymers.com All Rights Reserved