Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 113.8 MPa | 16510 psi | |
Abatron AboCast 8103-11 One Part Epoxy One component system. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 190 min. at 100°C (212°C). Peak exotherm 170°C (340°F). At.. |