Compressive Yield Strength 89.6 - 159 MPa
13000 - 23100 psi
Average value: 119 MPa Grade Count:8
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..