Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1060 MPa @Temperature 23.0 °C |
154000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® M10E Epoxy Resin, Carbon Tapes M10E 37%; Fiber: AS3C-S 300 GSMInformation provided by HexCel |