Hexcel® HexPly® M10E Epoxy Resin, Carbon Tapes

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M10E Epoxy Resin, Carbon Tapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
M10E 37%; Fiber: AS3C-S 300 GSMInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2020 MPa

@Temperature 23.0 °C
293000 psi

@Temperature 73.4 °F
Elongation at Yield 0.91 %

@Temperature 23.0 °C
0.91 %

@Temperature 73.4 °F
1.54 %

@Temperature 23.0 °C
1.54 %

@Temperature 73.4 °F
Tensile Modulus 121 GPa

@Temperature 23.0 °C
17600 ksi

@Temperature 73.4 °F
Compressive Yield Strength 1060 MPa

@Temperature 23.0 °C
154000 psi

@Temperature 73.4 °F
Compressive Modulus 117 GPa

@Temperature 23.0 °C
17000 ksi

@Temperature 73.4 °F