Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 154.9 MPa | 22470 psi | ASTM D695 |
Plenco 50240 PET, Pellet, Injection Molded, Blue
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |