Mechanical Properties Metric English Comments
Compressive Yield Strength 10.0 - 10.5 MPa

@Strain 1.00 %
1450 - 1520 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel
PTFE G Special Compound with steelInformation provided by Guarniflon®