Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1.02 MPa | 148 psi | at 30% deflection; ASTM D3574C |
Mearthane Durethaneâ„¢ F DF-245A Closed Cell Foam Polyurethane TDI backbone: ester.Shore 00 Hardness: 90Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |