Mechanical Properties Metric English Comments
Compressive Yield Strength 10.1 MPa
1460 psi
ASTM D695
3M Dyneon™ CC144/S PTFE, 40% Bronze Filled  (discontinued **)
Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon.