Material Notes:
Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 3.13 g/cc
0.113 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
value after 15 sec; ASTM D2240
67
67
initial value; ASTM D2240
Tensile Strength, Ultimate 22.8 MPa
3310 psi
ASTM D4745
Elongation at Break 250 %
250 %
ASTM D4894
Flexural Yield Strength <= 35.0 MPa
<= 5080 psi
ASTM D790
Compressive Yield Strength 10.1 MPa
1460 psi
ASTM D695
Compressive Modulus 0.460 GPa
66.7 ksi
ASTM D695
Coefficient of Friction, Dynamic 0.23
0.23
ASTM D3702
Coefficient of Friction, Static 0.21
0.21
ASTM D3702
K (wear) Factor 32.0 x 10-8 mm³/N-M
15.9 x 10-10 in³-min/ft-lb-hr
at 5000 psi - fpm PV; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
Copyright © lookpolymers.com All Rights Reserved