Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 91.01 MPa | 13200 psi | |
Abatron AboCast 8-16/Abocure 8-16 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/35.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 57 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless ca.. |
|||
Compressive Yield Strength | 91.0 MPa | 13200 psi | ASTM D695 |
Devcon Wear Guard (High Temp) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Compressive Yield Strength | 91.0 MPa | 13200 psi | |
Phenolic 27%, Graphite fabric 73% Phenolic - "91LD". Graphite fabric - "WCB" |