Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0600 MPa | 8.70 psi | at 10% deflection; ASTM D3574C |
Mearthane Durethaneâ„¢ M DM-715A Foam Polyurethane MDI backbone: ether.Shore 00 Hardness: 60Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Compressive Yield Strength | 0.0600 MPa @Strain 25.0 % |
8.70 psi @Strain 25.0 % |
ISO 7214 |
Zotefoams ZOTEK® F OSU Flexible PVDF Foam Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and .. |
|||
Compressive Yield Strength | 0.0600 MPa @Strain 25.0 % |
8.70 psi @Strain 25.0 % |
ISO 7214 |
Zotefoams ZOTEK® F 35 PVDF Foam Zotek® F 35 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |