Polymer Property : Compressive Yield Strength = 0.00800 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.00800 - 0.170 MPa
1.16 - 24.7 psi
Average value: 0.0627 MPa Grade Count:19
Overview of materials for Silicone Foam
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW..
Compressive Yield Strength 0.00800 MPa

@Strain 25.0 %
1.16 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Siliconcell 414/0 Silicone Foam
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.