Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 28.0 kN/m | 160 pli | TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Trefsin® 3101-75 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |
|||
Graves Tear Strength | 28.0 kN/m | 160 pli | TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Trefsin® 3201-75 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Graves Tear Strength | 28.0 kN/m @Temperature 23.9 °C |
160 pli @Temperature 75.0 °F |
Die C; ASTM D624 |
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Graves Tear Strength | 28.0 kN/m @Temperature 23.9 °C |
160 pli @Temperature 75.0 °F |
Die C; ASTM D624 |
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Graves Tear Strength | 28.0 kN/m | 160 pli | Die C; ASTM D624 |
Advanced Polymer Alloys DURACRYN 8060 NC/BK Thermoplastic Rubber Information provided by Advanced Polymer Alloys |
|||
Graves Tear Strength | 28.0 kN/m @Temperature 23.9 °C |
160 pli @Temperature 75.0 °F |
Die C; ASTM D624 |
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Graves Tear Strength | 28.0 kN/m | 160 pli | Die C; ASTM D642-54 |
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Gum Compound
(discontinued **)& Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Physical property data below (.. |
|||
Graves Tear Strength | 28.0 kN/m | 160 pli | Die C; ASTM D642-54 |
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Gum Compound
(discontinued **)& Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Reinforcing fillers not needed.. |
|||
Graves Tear Strength | 28.0 - 220 kN/m | 160 - 1260 pli | Average value: 112 kN/m Grade Count:15 |
Overview of materials for Chlorosulfonated Polyethylene Rubber This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val.. |