Polymer Property : Graves Tear Strength = 160 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 28.0 kN/m
160 pli
TPE-0056 (ASTM D 624)
Advanced Elastomer Systems Trefsin® 3101-75 W305 Thermoplastic Rubber  (discontinued **)
A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec..
Graves Tear Strength 28.0 kN/m
160 pli
TPE-0056 (ASTM D 624)
Advanced Elastomer Systems Trefsin® 3201-75 W305 Thermoplastic Rubber  (discontinued **)
A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t..
Graves Tear Strength 28.0 kN/m

@Temperature 23.9 °C
160 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 28.0 kN/m

@Temperature 23.9 °C
160 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 28.0 kN/m
160 pli
Die C; ASTM D624
Advanced Polymer Alloys DURACRYN 8060 NC/BK Thermoplastic Rubber
Information provided by Advanced Polymer Alloys
Graves Tear Strength 28.0 kN/m

@Temperature 23.9 °C
160 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 28.0 kN/m
160 pli
Die C; ASTM D642-54
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Gum Compound  (discontinued **)&
Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Physical property data below (..
Graves Tear Strength 28.0 kN/m
160 pli
Die C; ASTM D642-54
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Gum Compound  (discontinued **)&
Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Reinforcing fillers not needed..
Graves Tear Strength 28.0 - 220 kN/m
160 - 1260 pli
Average value: 112 kN/m Grade Count:15
Overview of materials for Chlorosulfonated Polyethylene Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val..