Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 9300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 64.1 MPa
9300 psi
ASTM D790
Polymer Resources ABS-GP1 General Purpose ABS
General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Flexural Strength 64.1 MPa
9300 psi
ASTM D790
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 64.1 MPa
9300 psi
ASTM D790
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade
General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Flexural Strength 64.1 MPa
9300 psi
ASTM D790
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized
General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In..
Flexural Strength 64.1 MPa

@Thickness 3.17 mm
9300 psi

@Thickness 0.125 in
ASTM D790
PTS Trilac® FR1 ABS- Flame Retardant ABS Resin  (Unverified Data**)
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Strength 64.1 MPa
9300 psi
ASTM D790
Techmer ES Plaslube® AC-80/TF/10 NAT Acetal (POM) Copolymer
Flexural Strength 64.1 MPa
9300 psi
ASTM D790
Techmer ES Plaslube® AC-80/TF/20 BK1941 Acetal (POM) Copolymer
Flexural Strength 64.1 MPa
9300 psi
ASTM D790
Techmer ES Plaslube® AC-80/TF/20 NAT Acetal (POM) Copolymer
Flexural Strength 64.1 MPa
9300 psi
Method I (3 point load), 1.3 mm/min; ASTM D790
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
Flexural Strength 64.1 MPa
9300 psi
ASTM D638
Plastics Group Polifil® GFRMPPCC-20 20% Glass Reinforced Polypropylene, High Impact
Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap..
Flexural Strength 64.1 MPa
9300 psi
ASTM D790B
Chevron Phillips EA3400 Medium Flow Crystal
DescriptionChevron EA3400 is a medium flow-crystal polystyrene resin developed to blend with Styrene-Butadiene block copolymers for sheet extrusion and vacuum thermoforming. EA3400 can be used in c..