Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® FD-1122 PC, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® TF-0930 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® FD-1122 PC, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® TF-0930 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | ASTM D790 |
E-Polymers TEKALOY® G70NHT Non Halogen Flame Retardant Impact Resistance PC/ABS Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | ASTM D790 |
Beijing Ranger Chem BLUESTAR® BS450 Acetal Copolymer Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60T6F Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Strength | 93.2 MPa | 13500 psi | ASTM D790 |
Beijing Ranger Chem BLUESTAR® BS350 Acetal Copolymer Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |