Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 92.5 MPa | 13400 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L6180 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |