Polymer Property : Flexural Strength = 9.50 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 9.50 MPa

@Temperature 120 °C
1380 psi

@Temperature 248 °F
ASTM Test
BASF Ultramid® HPN 9350 HS PA6 (Dry)
Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res..